Objective: Heat the bore of a hardened spur steel gear to shrink fit onto a gear motor shaft. This is part of a chair for the disabled.

Frequency: 300 kHz


Equipment:

  • Ambrell 2 kW induction heating system, equipped with a remote workhead containing two 0.66 μF capacitors for a total of 1.32 μF;
  • An induction heating coil designed and developed specifically for this application.

Material: Steel gear 2.5” (63.5mm) OD, .75” (19mm) ID x .625” (16mm) thick, temperature indicating paint

Temperature: 400 ºF (204 ºC)


Process:

A four turn helical internal coil is used to heat the gear bore. The coil is inserted into the gear bore and power is applied for 90 seconds to reach the required 400 ºF (204 ºC) and expand the gear bore. The gear is then placed on the shaft and allowed to cool, creating the shrink fit between the gear and the shaft.


Benefits:

  • No pre-heat cycle, heat is available on demand;
  • Energy efficient, heats only the part, not the atmosphere around it;
  • Controlled, even distribution of heating;
  • Faster production times.

Zašlete dotaz

Máte zájem o tento produkt? Potřebujete další informace nebo individuální ceny?

Kontaktujte nás
ZEPTEJTE SE O PRODUKT close
Děkujeme za zaslání zprávy. Odpovíme co nejdříve.
ZEPTEJTE SE O PRODUKT close
Procházet

Přidat do seznamu přání

musíš být přihlášen

Shrink fit a steel gear onto a motor shaft

Objective: Heat the bore of a hardened spur steel gear to shrink fit onto a gear motor shaft. This is part of a chair for the disabled.

Frequency: 300 kHz


Equipment:

  • Ambrell 2 kW induction heating system, equipped with a remote workhead containing two 0.66 μF capacitors for a total of 1.32 μF;
  • An induction heating coil designed and developed specifically for this application.

Material: Steel gear 2.5” (63.5mm) OD, .75” (19mm) ID x .625” (16mm) thick, temperature indicating paint

Temperature: 400 ºF (204 ºC)


Process:

A four turn helical internal coil is used to heat the gear bore. The coil is inserted into the gear bore and power is applied for 90 seconds to reach the required 400 ºF (204 ºC) and expand the gear bore. The gear is then placed on the shaft and allowed to cool, creating the shrink fit between the gear and the shaft.


Benefits:

  • No pre-heat cycle, heat is available on demand;
  • Energy efficient, heats only the part, not the atmosphere around it;
  • Controlled, even distribution of heating;
  • Faster production times.
Komentáře (0)