Objective: Annealing a 1” lip on aluminum cryogenic dewar* that has been work hardened during the process of spin forming.
Frequency: 303 kHz
Material: Aluminum dewar, lip has a 3.24” (82.3mm) ID and is 0.05” (1.3mm) thick.
Temperature: 800 °F (427 °C)
A two turn helical coil is used to heat the lip on the cryogenic dewar. The dewar is placed in the coil and power is applied for 2 minutes to anneal the required 1” heat zone.
Interessieren Sie sich für dieses Produkt? Benötigen Sie zusätzliche Informationen oder individuelle Preise?
Sie müssen eingeloggt sein
Objective: Annealing a 1” lip on aluminum cryogenic dewar* that has been work hardened during the process of spin forming.
Frequency: 303 kHz
Material: Aluminum dewar, lip has a 3.24” (82.3mm) ID and is 0.05” (1.3mm) thick.
Temperature: 800 °F (427 °C)
A two turn helical coil is used to heat the lip on the cryogenic dewar. The dewar is placed in the coil and power is applied for 2 minutes to anneal the required 1” heat zone.