Objective: To heat magnetic steel pins (spokes) for forging on a rim without heat treating and weakening the rim. Previously, a torch was utilized and the heating time was 20 seconds.


Frequency: 294 kHz


Equipment:
  • Ambrell EASYHEATTM 8310 LI, 10 kW induction heating system, equipped with a remote workhead containing one 1 μF capacitor;
  • A helical induction heating coil designed and developed specifically for this application.

Material: 9/16” (14 mm) steel pins.


Temperature: 2000 °F (1093 °C)


Process:

A single position three-turn helical coil was used, and the part was placed under the coil. The part was heated to the desired temperature within just seven seconds.


Benefits:
  • Fast, precise heating of the pin – 2 minutes and 36 seconds were saved on heating all of the rim’s pins when compared to using a torch;
  • The rim was not heated, which maintained its strength and durability;
  • Energy was saved due to the reduction in heating time;
  • There is more repeatability with induction when compared to using a torch.

Send an inquiry

Are you interested in this product? Do you need additional information or individual pricing?

Contact us
ASK FOR THE PRODUCT close
Thank you for sending your message. We will respond as soon as possible.
ASK FOR THE PRODUCT close
Browse

Add to Wishlist

You must be logged in

Preheating for Forging of Steel Pins


Objective: To heat magnetic steel pins (spokes) for forging on a rim without heat treating and weakening the rim. Previously, a torch was utilized and the heating time was 20 seconds.


Frequency: 294 kHz


Equipment:
  • Ambrell EASYHEATTM 8310 LI, 10 kW induction heating system, equipped with a remote workhead containing one 1 μF capacitor;
  • A helical induction heating coil designed and developed specifically for this application.

Material: 9/16” (14 mm) steel pins.


Temperature: 2000 °F (1093 °C)


Process:

A single position three-turn helical coil was used, and the part was placed under the coil. The part was heated to the desired temperature within just seven seconds.


Benefits:
  • Fast, precise heating of the pin – 2 minutes and 36 seconds were saved on heating all of the rim’s pins when compared to using a torch;
  • The rim was not heated, which maintained its strength and durability;
  • Energy was saved due to the reduction in heating time;
  • There is more repeatability with induction when compared to using a torch.