Recuit de l'extension de l'arbre du moteur hydraulique avant l'usinage

Annealing the end of a hydraulic motor shaft prior to machining


Objective: Annealing the end of a steel hydraulic motor shaft prior to machining.


Frequency: 259 kHz


Equipment:
  • Ambrell 4.2 kW induction heating system, equipped with a remote workhead containing one 1.0 μF capacitor;
  • A coil specifically designed for this application.

Material: 0.75” (19mm) diameter steel rod, 6” (152.4mm) long with a keyway at the end.


Temperature: 1350 °F (732 °C)


Process:

A three turn helical coil is used for annealing the motor shaft. The end of the motor shaft is placed in the coil and power is applied for 20 seconds to reach 1350 ºF (732 ºC) and turn the steel red hot.


Benefits:
  • High efficiency, low energy cost;
  • Precise and controllable placement of heat to anneal only the required area;
  • Faster production process;
  • Consistent results.

Envoyez une demande

Êtes-vous intéressé par ce produit? Avez-vous besoin d'informations supplémentaires ou d'une tarification individuelle?

Nous contacter
DEMANDEZ LE PRODUIT close
Merci d'avoir envoyé votre message. Nous vous répondrons dans les plus brefs délais.
DEMANDEZ LE PRODUIT close
Feuilleter

Ajouter à la liste de souhaits

Vous devez être connecté

Annealing the end of a hydraulic motor shaft prior to machining


Objective: Annealing the end of a steel hydraulic motor shaft prior to machining.


Frequency: 259 kHz


Equipment:
  • Ambrell 4.2 kW induction heating system, equipped with a remote workhead containing one 1.0 μF capacitor;
  • A coil specifically designed for this application.

Material: 0.75” (19mm) diameter steel rod, 6” (152.4mm) long with a keyway at the end.


Temperature: 1350 °F (732 °C)


Process:

A three turn helical coil is used for annealing the motor shaft. The end of the motor shaft is placed in the coil and power is applied for 20 seconds to reach 1350 ºF (732 ºC) and turn the steel red hot.


Benefits:
  • High efficiency, low energy cost;
  • Precise and controllable placement of heat to anneal only the required area;
  • Faster production process;
  • Consistent results.