Objective: To heat magnetic steel pins (spokes) for forging on a rim without heat treating and weakening the rim. Previously, a torch was utilized and the heating time was 20 seconds.
Frequency: 294 kHz
Material: 9/16” (14 mm) steel pins.
Temperature: 2000 °F (1093 °C)
A single position three-turn helical coil was used, and the part was placed under the coil. The part was heated to the desired temperature within just seven seconds.
Êtes-vous intéressé par ce produit? Avez-vous besoin d'informations supplémentaires ou d'une tarification individuelle?
Ajouter à la liste de souhaits
Vous devez être connecté
Objective: To heat magnetic steel pins (spokes) for forging on a rim without heat treating and weakening the rim. Previously, a torch was utilized and the heating time was 20 seconds.
Frequency: 294 kHz
Material: 9/16” (14 mm) steel pins.
Temperature: 2000 °F (1093 °C)
A single position three-turn helical coil was used, and the part was placed under the coil. The part was heated to the desired temperature within just seven seconds.