Plieninių kaiščių kaitinimas prieš kalimą

Preheating for Forging of Steel Pins


Objective: To heat magnetic steel pins (spokes) for forging on a rim without heat treating and weakening the rim. Previously, a torch was utilized and the heating time was 20 seconds.


Frequency: 294 kHz


Equipment:
  • Ambrell EASYHEATTM 8310 LI, 10 kW induction heating system, equipped with a remote workhead containing one 1 μF capacitor;
  • A helical induction heating coil designed and developed specifically for this application.

Material: 9/16” (14 mm) steel pins.


Temperature: 2000 °F (1093 °C)


Process:

A single position three-turn helical coil was used, and the part was placed under the coil. The part was heated to the desired temperature within just seven seconds.


Benefits:
  • Fast, precise heating of the pin – 2 minutes and 36 seconds were saved on heating all of the rim’s pins when compared to using a torch;
  • The rim was not heated, which maintained its strength and durability;
  • Energy was saved due to the reduction in heating time;
  • There is more repeatability with induction when compared to using a torch.

Atsiųskite užklausą

Ar Jūs domina šis produktas? Ar Jums reikia papildomos informacijos ar individualaus pasiūlymo?

Susisiekite su mumis
KLAUSKITE PRODUKTO close
Dėkojame, kad atsiuntėte žinutę. Atsakysime kuo greičiau.
KLAUSKITE PRODUKTO close
Naršyti

Pridėti į norų sąrašą

tu turi būti prisijungęs

Preheating for Forging of Steel Pins


Objective: To heat magnetic steel pins (spokes) for forging on a rim without heat treating and weakening the rim. Previously, a torch was utilized and the heating time was 20 seconds.


Frequency: 294 kHz


Equipment:
  • Ambrell EASYHEATTM 8310 LI, 10 kW induction heating system, equipped with a remote workhead containing one 1 μF capacitor;
  • A helical induction heating coil designed and developed specifically for this application.

Material: 9/16” (14 mm) steel pins.


Temperature: 2000 °F (1093 °C)


Process:

A single position three-turn helical coil was used, and the part was placed under the coil. The part was heated to the desired temperature within just seven seconds.


Benefits:
  • Fast, precise heating of the pin – 2 minutes and 36 seconds were saved on heating all of the rim’s pins when compared to using a torch;
  • The rim was not heated, which maintained its strength and durability;
  • Energy was saved due to the reduction in heating time;
  • There is more repeatability with induction when compared to using a torch.